Case Study

Die-Casting Mold Insert with Conformal Cooling

Die-Casting Mold Insert with Conformal Cooling

Pages 6 Pages

EQUIPMENT | POWDER | SOFTWARE | CONSULTING | SERVICE | SLM-SOLUTIONS.COM Optimizing tool construction and die-casting processes at Oskar Frech Case Study Die-Casting Mold Insert with Conformal Cooling GERMANY | CHINA | FRANCE | INDIA | ITALY | RUSSIA | SINGAPORE | USA | SLM-SOLUTIONS.COM60% SHORTER COOLING TIMES through internal cooling channels Part Data Designation: Core for a die casting mold Industry: Tooling Material: 1.2709 Layer Thickness: 40 µm Build Time: 1d 7h Machine: SLM®280 PROCESS OPTIMIZATION to reduce overall cycle times INCREASED SERVICE LIFE with optimized tempering 3D-Printing Success StoryFor tempering (heating and