Case Study

Level 3 Industrial Case Study Material Properties and Selection of Superalloys

Level 3 Industrial Case Study Material Properties and Selection of Superalloys

Pages 6 Pages

EDUCATION RESOURCES © 2021 ANSYS, Inc. Claes Fredriksson and Luca Masi Ansys Education Division Level 3 Industrial Case Study Material Properties and Selection of SuperalloysGRANTA EDUPACK © 2021 ANSYS, Inc. 2 Material properties of superalloy blades Superalloys are high-performance metal alloys that exhibit excellent mechanical properties such as strength and creep resistance at elevated temperatures. They generally display good surface stability as well as durability to corrosion and oxidation. It is not surprising then that they have found extensive use in demanding aerospace, automotive and marine applications. They are also common in chemical processing industry. The three main types are Nickel base, Nickel-Iron, and Cobalt base super-alloys, all with various specific con

Join for free to read