CASE STUDY INVESTMENT CASTING Size: 32 lbs | Alloy: CF8M *Notes: This one-piece casting eliminated the need for costly and time-consuming fabrication. Pipe Pushing Block The original casting design had a feature that was too thick creating clearance issues when assembled with the mating part. The permanent fix for the casting would be to modify the tool, but due to costliness of the tool modification as well as the time frame in w